Physical Properties Metric English Comments
ESCR 10% Igepal® 0.50 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
0.50 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Braskem IJ33D LLDPE Injection Molding Polyethylene Copolymer
IJ33D is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, excellent flexibi..