Polymer Property : ESCR 10% Igepal® = 10000 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
ESCR 10% Igepal® >= 10000 hour
>= 10000 hour
ASTM D1693-A
Borealis Borstar® HE3490-LS Black High Density Polyethylene for Pressure Pipes
Borstar HE3490-LS is a black, bimodal, high density polyethylene classified as an MRS 10.0 material (PE100) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding..