Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 240 hour | 240 hour | F50; ASTM D1693B |
ExxonMobil LLDPE LL 6407.67 Linear Low Density Polyethylene Resin Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processabi.. |