Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 28 hour @Thickness 2.00 mm, Temperature 50.0 °C |
28 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem ML4400N LLDPE Rotomolding Polyethylene The resin ML4400N is a linear low-density polyethylene, 1-butene based, with high stiffness and an adequate balance of processability and environmental stress cracking resistance. It contains long t.. |