Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | >= 500 hour | >= 500 hour | Condition B; ASTM D1693 |
Formosa Plastics Formolene® E900 Pipe HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin for Non-Pressure Pipe Extrusion Applications Formolene® E900 is a high molecular weight high density polyethylene (HMW-HDPE) resin des.. |
|||
ESCR 10% Igepal® | 500 hour | 500 hour | Condition A, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L64220U Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L64220U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase ProcessTM. Th.. |