ESCR 10% Igepal® 55 hour
55 hour
ASTM D1693
ExxonMobil LL 8555.67 Rotational Molding Resin  (discontinued **)
LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir..