Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.0714 cc-mm/m²-24hr-atm | 0.181 cc-mil/100 in²-24hr-atm | or 1.4 g/m²/atm/24 hr |
Dow ATTANE™ 4213 Ultra Low Density Polyethylene ATTANE® 4213 copolymer is an ultra low density polyethylene that offers excellent flexibility, sealability, puncture resistance and superior strength. It exhibits oxygen transmission characteristic.. |