Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.140 cc-mm/m²-24hr-atm | 0.356 cc-mil/100 in²-24hr-atm | ASTM F1249 |
Chevron Phillips HiD® 9650 HDPE Blown Film Resin
(discontinued **) Resin Type: Linear Polyethylene CopolymerCharacteristics: Copolymerization Enhances Film Toughness, Excellent Film Drawdown, Unique Molecular Architecture Gives Moisture Barrier Properties Typical o.. |
|||
Moisture Vapor Transmission | 0.140 cc-mm/m²-24hr-atm | 0.356 cc-mil/100 in²-24hr-atm | Proc. E; ASTM E96 |
DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the op.. |
|||
Moisture Vapor Transmission | 0.140 cc-mm/m²-24hr-atm | 0.356 cc-mil/100 in²-24hr-atm | Proc. E; ASTM E96 |
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo.. |