Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.530 cc-mm/m²-24hr-atm | 1.35 cc-mil/100 in²-24hr-atm | Proc. E; ASTM E96 |
DuPont Teijin Films Mylar® LBT-2 Polyester Packaging Film, 48 Gauge Data provided by DuPont Packaging Polymers.Mylar® LBT-2 is an uncoated, transparent, exceptionally strong film used as a substrate for laminating and extrusion coating and as a component of packagi.. |