Polymer Property : Moisture Vapor Transmission = 0.550 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.550 cc-mm/m²-24hr-atm
1.40 cc-mil/100 in²-24hr-atm
at 14.2 lbs/ream coating (1.0 mil); ASTM E96-53T
Chevron Phillips MarFlex® 1013 LDPE Extrusion Coating Resin
Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down ResinApplications: Food Packaging, LaminationsData provided by Chevron Che..
Moisture Vapor Transmission 0.550 cc-mm/m²-24hr-atm
1.40 cc-mil/100 in²-24hr-atm
at 14.2 lbs/ream coating (1.0 mil); ASTM E96-53T
Chevron Phillips MarFlex® 1019 Extrusion Coating Resin
Resin Type: Very High Speed at Low Coating WeightsCharacteristics: Excellent Processability, Process at Lower Temperature, High Temperature Stability, Excellent Draw Down ResinApplications:Food Pack..