Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.900 cc-mm/m²-24hr-atm @Temperature 38.0 °C |
2.29 cc-mil/100 in²-24hr-atm @Temperature 100 °F |
100%RH; ASTM F 1249 |
SABIC Innovative Plastics Lexan® DMX2415 PC Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ.. |
|||
Moisture Vapor Transmission | 0.900 cc-mm/m²-24hr-atm @Temperature 38.0 °C |
2.29 cc-mil/100 in²-24hr-atm @Temperature 100 °F |
100%RH; ASTM F 1249 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P.. |
|||
Moisture Vapor Transmission | 0.900 cc-mm/m²-24hr-atm @Temperature 38.0 °C |
2.29 cc-mil/100 in²-24hr-atm @Temperature 100 °F |
100%RH; ASTM F 1249 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
Moisture Vapor Transmission | 0.900 cc-mm/m²-24hr-atm @Temperature 38.0 °C |
2.29 cc-mil/100 in²-24hr-atm @Temperature 100 °F |
100%RH; ASTM F 1249 |
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region. |