Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.591 cc-mm/m²-24hr-atm | 1.50 cc-mil/100 in²-24hr-atm | 37°C; 90% RH |
Parylene Coating Services N Poly (P-Xylylene) Monomer is para-xylylene. Parylene N has a lower coefficient of friction and therefore is recommended where lubricity is needed. Parylene N exhibits a slight haze at thicknesses over 5 microns.Par.. |
|||
Moisture Vapor Transmission | 0.590 - 0.940 cc-mm/m²-24hr-atm | 1.50 - 2.39 cc-mil/100 in²-24hr-atm | Average value: 0.789 cc-mm/m²-24hr-atm Grade Count:8 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Moisture Vapor Transmission | 0.590 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1.50 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
g-mm/m²-day; based on film thickness; ASTM E96; ASTM E96 |
DuPont Elvax® 3121A Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 7.5 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dr.. |
|||
Moisture Vapor Transmission | 0.590 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1.50 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
g-mm/m²-day; based on film thickness; ASTM E96; ASTM E96 |
DuPont Elvax® 3120 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 7.5 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dr.. |