Physical Properties Metric English Comments
Moisture Vapor Transmission 0.960 - 1.74 cc-mm/m²-24hr-atm
2.44 - 4.42 cc-mil/100 in²-24hr-atm
40°C- 90% RH; based on 30 µm layer
Noltex Soarnol® DC3212 Ethylene Vinyl Alcohol Copolymer
Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..