Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 3.42 - 4.18 cc-mm/m²-24hr-atm | 8.69 - 10.6 cc-mil/100 in²-24hr-atm | 38 µm film; DIN 53122 Part 1 |
Stanelco Bioplast® GF 106 Biodegradable Plastic Bioplast 106 is a versatile soft product, suitable for blown film extrusion of completely biodegradable products. Many customers find it is a natural replacement for LDPE. Made from potato starch m.. |