Polymer Property : Moisture Vapor Transmission = 2.41 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.950 cc-mm/m²-24hr-atm
2.41 cc-mil/100 in²-24hr-atm
ASTM 1249
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..