Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 1.00 cc-mm/m²-24hr-atm | 2.54 cc-mil/100 in²-24hr-atm | Cup Method,40°C- 90% RH; based on 30 µm layer |
Noltex Soarnol® BG3522 Ethylene Vinyl Alcohol Copolymer Special designed high MFI grade. New EVOH for extrusion coating. Ethylene content 35 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, .. |