Polymer Property : Moisture Vapor Transmission = 3.56 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 1.40 cc-mm/m²-24hr-atm
3.56 cc-mil/100 in²-24hr-atm
g-mm/m²-day; based on 1 mil (0.0254 mm) thick film; ASTM E96
DuPont Elvax® 3173SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film  (discontinued **)<
18 wt% Vinyl Acetate.Elvax® 3173SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res..