Moisture Vapor Transmission 1.50 cc-mm/m²-24hr-atm
3.81 cc-mil/100 in²-24hr-atm
40°C, 90% RH
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa..
Moisture Vapor Transmission 1.50 cc-mm/m²-24hr-atm
3.81 cc-mil/100 in²-24hr-atm
40°C, 90% RH
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan..
Moisture Vapor Transmission 1.50 cc-mm/m²-24hr-atm
3.81 cc-mil/100 in²-24hr-atm
40°C, 90% RH
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL..
Moisture Vapor Transmission 1.50 cc-mm/m²-24hr-atm
3.81 cc-mil/100 in²-24hr-atm
40°C, 90% RH
EVALCA EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applicat..
Moisture Vapor Transmission 1.50 cc-mm/m²-24hr-atm
3.81 cc-mil/100 in²-24hr-atm
g-mm/m²-day; based on 1 mil (0.0254 mm) thick film; ASTM E96
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
Moisture Vapor Transmission 1.50 cc-mm/m²-24hr-atm
3.81 cc-mil/100 in²-24hr-atm
42% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Dow Tyrin® 4211P Chlorinated Polyethylene Elastomer
42% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P..
Moisture Vapor Transmission 1.50 cc-mm/m²-24hr-atm
3.81 cc-mil/100 in²-24hr-atm
40°C, 90% RH
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro..
Moisture Vapor Transmission 1.50 cc-mm/m²-24hr-atm
3.81 cc-mil/100 in²-24hr-atm
40°C, 90% RH
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc..