Polymer Property : Carbon Dioxide Transmission = 1.20 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Carbon Dioxide Transmission 1.20 cc-mm/m²-24hr-atm
3.05 cc-mil/100 in²-24hr-atm
30°C, 1 atm for 24 Hours; ASTM D1434
UBE UPILEX 25S (25 micron) Polyimide Film
Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries..