Polymer Property : Carbon Dioxide Transmission = 149 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Carbon Dioxide Transmission 149 cc-mm/m²-24hr-atm
378 cc-mil/100 in²-24hr-atm
ASTM D1434
Eastman Tritan FX100 Copolyester
Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..
Carbon Dioxide Transmission 149 cc-mm/m²-24hr-atm
378 cc-mil/100 in²-24hr-atm
ASTM D1434
Eastman Tritan MP100 Copolyester
Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co..