Physical Properties Metric English Comments
Carbon Dioxide Transmission 1.38 cc-mm/m²-24hr-atm
3.50 cc-mil/100 in²-24hr-atm
80% RH, 23°C, oriented film
Honeywell Aegis™ OX High Barrier Nylon  (discontinued **)
Description: Aegis OX is an oxygen-scavenging nylon. Oxygen barrier is comparable to a glass bottle with metal crown closure. In addition Aegis OX provides CO2 barrier and possesses glass-like cla..