Physical Properties Metric English Comments
Carbon Dioxide Transmission 290 cc-mm/m²-24hr-atm
737 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® BM 17 PA*
Product description: Grilon BM 17 natural is a medium viscosity multi-polyamide with a low melting point. Grilon BM 17 natural has the following features: High flexibility and toughnessVery good ori..