Melt Density 0.884 g/cc
0.0319 lb/in³
Melt density
Americas Styrenics Styron® XL-8023VC High Impact Polystyrene  (discontinued **)
STYRON® XL-8023 VC high impact polystyrene is designed to provide molders of VCR cassettes with the impact and gloss they require, at economics and processability highly advantaged over ABS resins...
Melt Density 0.882 g/cc
0.0319 lb/in³
Melt density
Styron Magnumâ„¢ 9010 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..