Polymer Property : Melt Density = 0.962 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Density 0.962 g/cc
0.0348 lb/in³
Melt density
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced
PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used..
Melt Density 0.962 g/cc
0.0348 lb/in³
Melt density
Styron Pulse® 830 ABS + Polycarbonate
PULSE® 830 Engineering resin offers excellent processability, high heat resistance, and high impact strength at both room and low temperatures.PULSE 830 Engineering resin has been used in automot..