Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Density | 0.963 g/cc | 0.0348 lb/in³ | Melt density |
Dow AIM® 4800 High Impact Styrenic Resin AIM® 4800 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Melt Density | 0.963 g/cc | 0.0348 lb/in³ | Melt density |
Dow AIM® 4810 High Impact Styrenic Resin AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |