Polymer Property : Melt Density = 0.965 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Density 0.965 g/cc
0.0349 lb/in³
Melt density
Americas Styrenics Styron® 425 High Impact Polystyrene  (discontinued **)
STYRON® 425 impact polystyrene resin is typically used in thin section parts, hot drink cups and cassettes. It offers heat resistance, easy flow, fast cycling, and excellent tensile and flex proper..