Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Density | 1.00 g/cc | 0.0361 lb/in³ | Melt density |
Styron CALIBRE™ 300 15 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Melt Density | 1.00 g/cc | 0.0361 lb/in³ | Melt density |
Styron CALIBRE™ 300 4 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Melt Density | 1.00 g/cc | 0.0361 lb/in³ | Melt density |
Styron CALIBRE™ 300 6 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Melt Density | 1.00 g/cc | 0.0361 lb/in³ | Melt density |
Styron Magnum™ 342EZ ABS, Medium Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Density | 1.00 g/cc | 0.0361 lb/in³ | Melt density |
Dow Tyril® 880B SAN TYRIL® 880B SAN copolymer combines the high levels of chemical resistance, heat resistance and overall strength of 880 resin with improved mold flow and mold release characteristics.Data provided b.. |