Polymer Property : Melt Index of Compound = 0.50 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 1012/0001 Polyvinylidene Fluoride  (discontinued **)
High molecular weight grade PVDFSuitable for compression molding or extrusionExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent stre..
Melt Index of Compound 0.50 g/10 min

@Load 10.0 kg,
Temperature 230 °C
0.50 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 1012/1001 Polyvinylidene Fluoride  (discontinued **)
High molecular weight grade PVDFPowder gradeExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabilityInf..
Melt Index of Compound <= 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
<= 0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow Engage® ENR 7086.01 Ethylene-Butene Copolymer
Description: ENR 7086.01 is a revolutionary new ethylene-butene copolymer with a broader molecular weight distribution and much higher levels of long chain branching than other commercially availabl..
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 6012/0000 Polyvinylidene Fluoride
3M™ Dyneon™ PVDF 6012/0000 is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, and ..