Physical Properties Metric English Comments
Melt Index of Compound 19 g/10 min

@Load 2.16 kg,
Temperature 260 °C
19 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CX7259 PC (Asia Pacific)
Cycoloy resin grade CX7259 is a flame retardant impact modified polycarbonate blend aiming at ultra thin wall designs. It is listed as UL-94 V1 at 0.5mm & V0 at 0.6mm with excellent flow and balance..
Melt Index of Compound 19 g/10 min

@Load 2.16 kg,
Temperature 250 °C
19 g/10 min

@Load 4.76 lb,
Temperature 482 °F
cm3/10 min; ISO 1133
DuPont Performance Polymers Crastin® SK615SF NC010 PBT  (Unverified Data**)
Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc..
Melt Index of Compound 19 g/10 min

@Load 2.16 kg,
Temperature 250 °C
19 g/10 min

@Load 4.76 lb,
Temperature 482 °F
cm3/10 min; ISO 1133
DuPont Performance Polymers Crastin® SK615SF NC010 PBT  (Unverified Data**)
Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc..
Melt Index of Compound 19 g/10 min

@Load 2.16 kg,
Temperature 250 °C
19 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East)
VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications.
Melt Index of Compound 19 g/10 min

@Load 5.00 kg,
Temperature 265 °C
19 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
Melt Index of Compound 19 g/10 min

@Load 5.00 kg,
Temperature 265 °C
19 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.