Melt Index of Compound 23 g/10 min

@Load 5.00 kg,
Temperature 300 °C
23 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL PX9406P PPE+HIPS (Asia Pacific)
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 125dc HDT. UL94 V-0 rated. Electrical applications.
Melt Index of Compound 23 g/10 min

@Load 5.00 kg,
Temperature 250 °C
23 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East)
VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles.
Melt Index of Compound 23 g/10 min

@Load 5.00 kg,
Temperature 250 °C
23 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East)
VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles.
Melt Index of Compound 23 g/10 min

@Load 5.00 kg,
Temperature 265 °C
23 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East)
VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage.
Melt Index of Compound 23 g/10 min

@Load 5.00 kg,
Temperature 250 °C
23 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
Melt Index of Compound 23 g/10 min

@Load 5.00 kg,
Temperature 250 °C
23 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East)
VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles.