Polymer Property : Melt Index of Compound = 25 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 25 g/10 min

@Load 5.00 kg,
Temperature 260 °C
25 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific)
UV stabilized, non-FR PC/ABS of excellent flow and impact performance
Melt Index of Compound 25 g/10 min

@Load 5.00 kg,
Temperature 265 °C
25 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® XCY620HS PC+ABS
PC+ ABS General Purpose Non-FR
Melt Index of Compound 25 g/10 min

@Load 5.00 kg,
Temperature 265 °C
25 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS
PC+ ABS Automotive applications
Melt Index of Compound 25 g/10 min

@Load 5.00 kg,
Temperature 265 °C
25 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Europe-Africa-Middle East)
PC+ ABS automotive applications, excellent flow/impact balance, high heat resistance temperature and excellent properties retention after hydrolytic and heat aging.
Melt Index of Compound 25 g/10 min

@Load 5.00 kg,
Temperature 260 °C
25 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS
UV stabilized, non-FR PC/ABS of excellent flow and impact performance
Melt Index of Compound 25 g/10 min

@Load 5.00 kg,
Temperature 360 °C
25 g/10 min

@Load 11.0 lb,
Temperature 680 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics ULTEM 1010 PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant.
Melt Index of Compound 25 g/10 min

@Load 5.00 kg,
Temperature 360 °C
25 g/10 min

@Load 11.0 lb,
Temperature 680 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics ULTEM HU1010 PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), ..
Melt Index of Compound 25 g/10 min

@Load 5.00 kg,
Temperature 265 °C
25 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend
Melt Index of Compound 25 g/10 min

@Load 5.00 kg,
Temperature 250 °C
25 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East)
10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.
Melt Index of Compound 25 g/10 min

@Load 5.00 kg,
Temperature 265 °C
25 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East)
VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry.