Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 26 g/10 min @Load 2.16 kg, Temperature 250 °C |
26 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Crastin® SK612SF NC010 PBT
(Unverified Data**) Crastin® SK612SF is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Melt Index of Compound | 26 g/10 min @Load 2.16 kg, Temperature 250 °C |
26 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Crastin® SK612SF NC010 PBT
(Unverified Data**) Crastin® SK612SF is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Melt Index of Compound | 26 g/10 min @Load 2.16 kg, Temperature 280 °C |
26 g/10 min @Load 4.76 lb, Temperature 536 °F |
ISO 1133 |
Honeywell Aegis™ HFX High Barrier Nylon
(discontinued **) Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is .. |
|||
Melt Index of Compound | 26 g/10 min @Load 2.16 kg, Temperature 280 °C |
26 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East) Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par.. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® X2420 PC+POLYESTER (Asia Pacific) Xenoy*X2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad co.. |