Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML3729 PC Excellent flow, UV stabilized, grade which contains a release agent to ensure easy processing. |
|||
Melt Index of Compound | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML3729 PC (Europe-Africa-Middle East) LEXAN ML3729 is an UV stabilized grade, with an excellent flow. It contains a release agent to ensure easy processing. |