Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 44 g/10 min @Load 5.00 kg, Temperature 300 °C |
44 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FST9436 PC Copolymer Medium viscosity opaque, low smoke, and OSU 65/65 compliant PC Copolymer |