Physical Properties Metric English Comments
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific)
UV stabilized, non-FR PC/ABS of excellent flow and impact performance
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
Melt Index of Compound 8.0 g/10 min

@Load 5.00 kg,
Temperature 260 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics GELOY FXW710SK ASA
General purpose injection molding ASA with Visual Fx sparkle effect.
Melt Index of Compound 8.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
8.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics GELOY HRA170D ASA+PC (Europe-Africa-Middle East)
GELOY HRA170D resin is a PC-ASA blend with permanent antistatic behavior. It is typically used in applications that require antidust properties and high impact retention. Geloy HRA170D resin is typi..
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1200HF is the improved version of CYCOLOY C1200 and has been developed to provide enhanced productivity and surface appearance for
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS
UV stabilized, non-FR PC/ABS of excellent flow and impact performance
Melt Index of Compound 8.0 g/10 min

@Load 5.00 kg,
Temperature 260 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics GELOY CR7020 ASA (Europe-Africa-Middle East)
GELOY CR7020 is a profile extrusion and co-extrusion grade, blend of ASA/SAN. In co-extrusion it can be used over CYCOLAC, PVC or other compatible polymers.
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 1008/0001 Polyvinylidene Fluoride  (discontinued **)
Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an..
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Melt Index of Compound 8.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East)
VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures.
Melt Index of Compound 8.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East)
VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin.
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Melt Index of Compound 8.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Melt Index of Compound 8.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Asia Pacific)
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® 4512 PBT+PC (Europe-Africa-Middle East)
10% GF FR PBT/PC Blend
Melt Index of Compound 8.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Melt Index of Compound 8.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Europe-Africa-Middle East)
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 11008/0001 Polyvinylidene Fluoride
PVDF is ideal for multiple applications across a wide array of industries. Widely used in the chemical processing, wire and cable, semiconductor, and oil and gas industries. PVDF is also gaining rec..
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 11008/0003 Polyvinylidene Fluoride
PVDF is ideal for multiple applications across a wide array of industries. Widely used in the chemical processing, wire and cable, semiconductor, and oil and gas industries, PVDF is also gaining rec..
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 6108/0001 Polyvinylidene Fluoride
Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an..
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
3M Dyneon™ PVDF 6008/0001 Polyvinylidene Fluoride
Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an..
Copyright © lookpolymers.com All Rights Reserved