Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 1.6 - 1.7 cP | 1.6 - 1.7 cP | LCL-PR21 |
Intercontinental Polymers 552 PBT Polymer Type - Elastomer, Polyester Resin Applications: Engineering Resin - ModifiedInformation provided by Intercontinental Polymers. |