Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 2.54 cP | 2.54 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ FIT E 52 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® FIT E 52 is a high molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and reduc.. |