Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Relative Viscosity 2.83 cP
2.83 cP
QC-10-104
Formosa Plastics Formolon® 1071 PVC
PVC Homopolymer Dispersion Resin F-1071 is a high molecular weight, fine particle size PVC homopolymer dispersion resin with low surfactant content. The high molecular weight results in product with..