Physical Properties Metric English Comments
Relative Viscosity 3.71 - 3.89 cP
3.71 - 3.89 cP
96% H2SO4
UBE 7034B Nylon 6/12 Copolymer Film
Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal ..