Physical Properties Metric English Comments
Relative Viscosity 44 - 48 cP
44 - 48 cP
ASTM D789
Ascend Performance Materials Vydyne® 21Z Nylon 66, General Purpose
Vydyne® 21Z is a general-purpose PA66 resin. It is available in natural and designed for extrusion-compounding applications. This resin offers a well balance combination of engineering properties c..