Polymer Property : Storage Temperature = 59.0 °F Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Storage Temperature 15.0 - 25.0 °C
59.0 - 77.0 °F
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane
Pearlbondâ„¢ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo..
Storage Temperature 15.0 - 25.0 °C
59.0 - 77.0 °F
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane
Pearlbondâ„¢ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ..