Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 151 g/l | 151 g/l | |
Parker Chomerics CHO-BOND 1030 Conductive Silicone Gasket Adhesive Electrically conductive one-component silicone-based RTV adhesive which greatly simplifies the problem of bonding conductive silicone EMI gaskets to metal substrates. This adhesive cures on exposure.. |
|||
Volatile Organic Compounds (VOC) Content | 151 g/l | 151 g/l | |
Parker Chomerics CHO-BOND 1035 Electrically Conductive Sealant Electrically conductive, one component RTV silicone which provides both environmental sealing and EMI/RFI shielding. This sealant, filled with silver-plated glass particles, contains no acetic acid,.. |