Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | <= 250 g/l | <= 250 g/l | VOC Less H2O and Exempt Solvents |
3M 1000 NS Fire Barrier Water Tight Sealants 3M Fire Barrier Water Tight Sealants 1000 NS and 1003 SL are ready-to-use, single component, neutral cure, silicone sealants that cure upon exposure to atmospheric humidity to form a flexible firest.. |
|||
Volatile Organic Compounds (VOC) Content | <= 250 g/l | <= 250 g/l | VOC Less H2O and Exempt Solvents |
3M IC 15WB+ Fire Barrier Sealant 3M Fire Barrier Sealant IC 15WB+ is a cost-effective, one-part, gun-grade, latex-based, intumescent firestop sealant that dries to form a monolithic firestop seal that also acts as a barrier to airb.. |
|||
Volatile Organic Compounds (VOC) Content | <= 250 g/l | <= 250 g/l | VOC Less H2O and Exempt Solvents |
3M FD 150+ Fire Barrier Sealant 3M Fire Barrier Sealant FD 150+ is an economical, ready to use, gun-grade, elastomeric sealant that dries to from a monolithic flexible firestop seal. 3M Fire Barrier Sealant FD 150+ firestops joint.. |
|||
Volatile Organic Compounds (VOC) Content | <= 250 g/l | <= 250 g/l | VOC Less H2O and Exempt Solvents |
3M FIP 1-Step Fire Barrier Rated Foam 3M Fire Barrier Rated Foam (FIP 1-Step), is a smoke, sound, and firestopping foam for wall and floor penetrations. Premium two-part, easy-to-handle formulations. Expands up to five times during inst.. |
|||
Volatile Organic Compounds (VOC) Content | <= 250 g/l | <= 250 g/l | VOC Less H2O and Exempt Solvents |
3M 1003 SL Fire Barrier Water Tight Sealants 3M Fire Barrier Water Tight Sealants 1000 NS and 1003 SL are ready-to-use, single component, neutral cure, silicone sealants that cure upon exposure to atmospheric humidity to form a flexible firest.. |
|||
Volatile Organic Compounds (VOC) Content | <= 250 g/l | <= 250 g/l | VOC Less H2O and Exempt Solvents |
3M SS100 Smoke and Sound Sealant 3M Smoke and Sound Sealant SS 100 is an economical, ready to use, gun-grade, elastomeric sealant that drives to form a monolithic flexible seal that helps prevent unwanted noise infiltration and mit.. |