Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 0.000 - 33.0 g/l
0.000 - 33.0 g/l
Average value: 5.50 g/l Grade Count:6
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va..