Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 4.27 g/l
4.27 g/l
Tra-Con Tra-Cast 3108 General Purpose Epoxy Casting Compound
TRA-CAST 3108 is a low viscosity two-part formulation recommended for underfill and encapsulating applications where the combination of good mechanical thermal and electrical properties are required..