Polymer Property : Volatile Organic Compounds (VOC) Content = 504 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 504 g/l
504 g/l
3M Super 77™ Spray Adhesive
A high tack, high coverage and fast drying adhesiveFeatures:A high tack, high coverage fast drying, transparent adhesive for permanently attaching foils, carpeting, many lightweight foams, permanent..