Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 680 g/l
680 g/l
Parker Chomerics CHO-SHIELD® 4914 Conductive Coating
Conductive Solvent-Resistant Acrylic Coating. Formulated for high resistance to solvent attack, CHO-SHIELD® 4914 is an electrically conductive, one-component acrylic coating. Compared to zinc arc s..