Polymer Property : Volatile Organic Compounds (VOC) Content = 70 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 70 g/l
70 g/l
EPA 24
Chesterton ARC NVE VC Vinyl Ester Sealer
Description: ARC NVE VC (Veil Coat) is a two-component, modified epoxy novolac vinyl ester sealer coat formulated for application by brush, roller or spray at 0.15-0.25 mm (0.07-0.010”) wet film th..