Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 9.03 g/l | 9.03 g/l | |
Tra-Con Tra-Bond F114BK01 Low Viscosity Blush-Free Epoxy Adhesive TRA-BOND F114BK01 is a low viscosity, room temperature cure, epoxy system that contains no solvents, has excellent wicking and wetting characteristics, and adheres strongly to glass, ceramics, most .. |
|||
Volatile Organic Compounds (VOC) Content | 9.03 g/l | 9.03 g/l | |
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive TRA-BOND F114 is a clear, low viscosity, room temperature cure, epoxy system with good optical properties that contains no solvents, has excellent wicking and wetting characteristics, and adheres st.. |