Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.676 g/cc @Temperature 288 °C |
0.0244 lb/in³ @Temperature 550 °F |
|
Duratherm 600 Paraffinic Heat Transfer Fluid Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to .. |
|||
Density | 0.676 g/cc @Temperature 288 °C |
0.0244 lb/in³ @Temperature 550 °F |
|
Duratherm 630 Paraffinic Heat Transfer Fluid Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F.. |